* '''Bottom layer:'''..Glass
Within this last specification mentioned above, the 2 thermoplastic layers together with the LED Interlayer will reach a total thickness of about 2mm. The usually very economical PVB is the most used [[Laminated glass|lamination interlayer]]. Its lamination is based on a nip roller pre-heating step followed by an autoclaving process with a final stage ideally below 125 °C and 14 athmospheres. However, polyester has a better adhesion to [[Thermoplastics polyurethanes (TPU)|TPU]], to [[Ethylene-vinyl acetate|EVA]] or to EVASafe